What to do with uneven morphology of pre stretched foam in blister processing

1. The blister processed sheet material is not evenly heated, and should be slowly heated or equipped with a heat shielding mesh;
2. The thickness of the sheet is uneven, and a sheet with uniform thickness should be replaced;
3. The distribution of blowing air pressure is uneven, and the airflow should be homogenized to ensure a uniform distribution of air pressure.